http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114214717-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_96dfcf8c09195e0d71955cbf6d71cc42 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25F3-20 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25F3-20 |
filingDate | 2021-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_189d9abd172bf6fb0f1e28658257f402 |
publicationDate | 2022-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-114214717-A |
titleOfInvention | A kind of aluminum alloy processing solution and preparation method thereof |
abstract | The invention provides an aluminum alloy processing solution. By configuring the solution containing perchloric acid, maleic acid, oxalic acid, rhodin, sulfosalicylic acid, butylene glycol, triethanolamine, phenylpropyltriazole, The electrolytic polishing solution of ethanol and water can effectively reduce the resistivity of the mucosa formed by the anodic dissolution process, improve the diffusivity of dissolved metals, and the surface roughness of the aluminum alloy is low, and the mirror effect is good. |
priorityDate | 2021-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 37.