http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114133513-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_abf51b71252eac4a2ec7edfd7152256a |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2150-90 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6415 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4081 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-5024 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-02 |
filingDate | 2021-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_91912ed4be1462985b0b84854a73e4d4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ef9405e4bdd869888bba94181a24321 |
publicationDate | 2022-03-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-114133513-A |
titleOfInvention | A kind of water-based polyaspartic acid ester dispersion, its preparation method and water-based polyurea coating resin |
abstract | The invention belongs to the technical field of coatings, and in particular relates to an aqueous polyaspartate dispersion, a preparation method thereof and an aqueous polyurea coating resin. The method includes steps: 1) dehydrating polyetheramine and polyaspartate resin at 100°C-120°C under negative pressure; 2) after step 1) is completed, cooling down to 20°C-60°C, dripping at a constant speed Add diisocyanate, the dropping time is controlled at 0.5h-1.5h, and the solvent is added, and after the dropping is completed, the temperature is raised to 40 ℃-80 ℃, and the reaction is held at a constant temperature; 3) After the completion of step 2), slowly add the preheated The ionized water was added dropwise for 0.5h-1.5h, then continued to be stirred for about 0.4h-0.6h, cooled down and discharged, to obtain the water-based polyaspartate dispersion. The water-based polyaspartate dispersion prepared by the invention has low VOC content, is safe, non-toxic and environmentally friendly, and the polyurea coating formed by compatibility with the water-based polyisocyanate has excellent comprehensive performance. |
priorityDate | 2021-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |