http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113930154-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_45d300003dec085c2641073fb639043b
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e2633103f98dbb84e9f96f1ebdf291d7
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8843e3dd4bf9369c8c560aeda0d4a41b
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-65
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-388
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-08
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-388
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65
filingDate 2021-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ecb61cfa469c00cc8e51cae8b9ed88f1
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ecb5e33c993a66eedccec669334da7d0
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a84c4f71b92848ec0c6885180eec3d2
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_21d234ba812597c36c3f7a0e2f5c1f91
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_861e3be895e4e248299ed27ba24a4d89
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ba71cc165088522768857f2ee22f4c9
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_314f49f0bd4a2b5df99d3dc55691d5e9
publicationDate 2022-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-113930154-A
titleOfInvention A kind of self-healing anti-pollution flashover coating and preparation method and application thereof
abstract The present invention provides a self-healing anti-pollution flashover coating and a preparation method and application thereof. The self-healing anti-pollution flashover coating comprises a combination of diamine-containing polydimethylsilane, a dinitrile monomer and a lubricant; Add diamine-containing polydimethylsilane as the base molecule, and add dinitrile monomers together, so that the two react to obtain a polymer containing hydrogen bond sites, which can form both intermolecular chains and intrachains. hydrogen bond, so that after the coating formed by the self-healing anti-pollution flashover coating is damaged, the molecular chain of the coating at the damaged position can move and re-form new hydrogen bonds, thereby repairing the damage; The coating can prevent the adhesion of pollutants and water droplets, and finally an anti-pollution flashover coating with high coating stability and self-healing performance is obtained.
priorityDate 2021-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017121624-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015037570-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2019367771-A1
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID21202
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559283
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419567101
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID8028

Total number of triples: 32.