http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113912948-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d6a6f422b091ba12ea61d4adbf1b0e8e
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-14
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-26
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-14
filingDate 2021-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2b01b555283bf5c3f0573e2a2e2eb0c
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65926227c5980fdf79bcb2040a4482b9
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_19b35b207d6f990d673a1bd18661d2e5
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eec3ba0bfaaf33ea6608831d63d6bf63
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef0dfd15b899dc32e0e4ba9a36b10602
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d613b88cc7432f12ef6349bc55ae31d3
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bcfbc0fcbe52d47bb8f6443e6315fb65
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b190f25c6b16588af517c65aa1bcf7a
publicationDate 2022-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-113912948-A
titleOfInvention Polypropylene nanocomposite with low temperature toughness and rigidity and preparation method thereof
abstract A polypropylene nanocomposite material with low temperature toughness and rigidity and a preparation method thereof, comprising the following components in parts by weight: 60-100 parts of polypropylene random copolymer, 15-33 parts of elastomer, 9-32 parts of inorganic rigid particles and 2-3 parts of polypropylene antioxidant, optionally 0.03-0.4 part of cross-linking agent can be added, and it is prepared by the traditional melt blending method, the process is simple and the process is few. The scheme of the present invention includes two modification methods: first, the elastomer and nano-silica coordinately adjust the brittle-ductile transition temperature of the material to achieve low temperature toughening; second, based on the dynamic vulcanization technology, the first modification method is optimized, Achieve low temperature toughening and rigid-tough balance of materials.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115044136-B
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115044136-A
priorityDate 2021-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5045589-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6325
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID10112
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID8285
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419593172
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID16703273
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID458393334
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559542
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID414859281
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707758
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID453467280
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6545
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419549665
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24261
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID104745
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID413807575

Total number of triples: 39.