http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113788977-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2205-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2471-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2471-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2423-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2325-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2375-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0066 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 |
filingDate | 2021-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-113788977-B |
titleOfInvention | A kind of preparation method of flexible porous material |
abstract | The present invention provides a kind of preparation method of flexible pore material, comprises the following steps: S1. 2-6 parts of surfactant, 1-3 parts of the first stabilizer are added to 30-40 parts of deionized water to prepare homogeneous The aqueous solution is used as the water phase; 5-20 parts of resin, 4-7 parts of propylene-styrene-butadiene copolymer, 1-3 parts of the second stabilizer, 3-5 parts of cell structure control agent, 1-4 parts Accelerator and 10-20 parts of diluent are prepared into a homogeneous oil solution as the oil phase; the water phase and the oil phase are quickly mixed to prepare an emulsion by homogeneous emulsification, stirring or ultrasonic method; S2. The prepared emulsion is polymerized, And filter, wash and dry, finally get the flexible porous material. According to the preparation method of the flexible porous material of the present invention, the average particle size of the foam microporous material prepared by the preparation method of the present invention is controllable, the cell structure is regular, the compression resilience is good, the flexibility is good, and the stability is excellent. |
priorityDate | 2021-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |