http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113652026-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8bff01e7c8abf83fd4071be9b12b3871 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-3045 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-329 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2206 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-523 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 |
filingDate | 2021-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_48b7dd6d1218c149135b51827447f906 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f9df49050c192c27d8c7c18c82b60f8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_35595088bfa28df4d1a7c8824066b9e5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81c625fe6507259935c9f92001f818b1 |
publicationDate | 2021-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-113652026-A |
titleOfInvention | Anti-reflection toughened high-isotatic PP material and preparation method thereof |
abstract | The invention discloses an anti-reflection toughened high isotactic PP material and a preparation method thereof, wherein the anti-reflection toughened high isotactic PP material comprises the following raw materials in parts by weight: 90-95 parts of polypropylene, 0.08-0.095 part of nucleating agent, 1-4 parts of stabilizing agent, 0.5-1 part of antioxidant, 0.001-0.95 part of flame retardant, 0.2-2 parts of alkyl peroxide, 0.04-0.2 part of toughening agent and 2-4 parts of transparent agent, wherein the ratio of the polypropylene to the nucleating agent is 1000:1, the peroxide is prepared by mixing hydrogen peroxide and dibenzoyl peroxide according to the ratio of 1:4, the ratio of the nucleating agent is prepared by mixing 2-6:4-6:6-9 of silicon dioxide, alum and calcium oxide, the ratio of the stabilizing agent is prepared by mixing 1-2:4-5:5-10 of zinc stearate, calcium carbonate and calcium hydroxide, various additives are added on a common PP material, and the transparency of the PP material can be improved by the nucleating agent and the transparent agent, the toughening agent can increase the toughness of the PP material, the stabilizing agent can increase the stability of the PP material in the preparation process, and the antioxidant can increase the service life of the PP material. |
priorityDate | 2021-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links