http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113372786-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1662 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F230-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F226-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-365 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-387 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-1804 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-1802 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F293-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D153-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D153-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F293-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F226-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F230-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-36 |
filingDate | 2021-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-113372786-B |
titleOfInvention | Method for preparing surface of antifouling material with microstructure |
abstract | The invention belongs to the field of marine antifouling, and relates to a method for preparing a surface of a microstructure antifouling material, which comprises the steps of preparing a hydrophobic macroinitiator, preparing a high-strength and high-toughness block polymer and preparing a porous microstructure antifouling surface, wherein the hydrophobic macroinitiator is prepared by using an organic silicon monomer, triethylamine, 2-bromoisobutyryl bromide and a solvent A, the high-strength and high-toughness block polymer with a hydrophobic chain segment and a hydrophilic chain segment which are alternately distributed is prepared by using the hydrophobic macroinitiator, a hydrophilic monomer, an acrylic monomer, a catalyst and a solvent B, and the high-strength and high-toughness block polymer is dissolved in a solvent C to prepare a solution, coated and dried to obtain the porous microstructure antifouling surface with high strength, strong hydrophobicity and good static antifouling performance; according to the preparation method, an organic silicon monomer, a hydrophilic monomer and an acrylic acid monomer are copolymerized, an acrylic acid chain segment is introduced to endow a block polymer with high toughness, and a hydrophilic and hydrophobic chain segment is utilized to spontaneously form a porous microstructure to endow the surface of the material with hydrophobicity. |
priorityDate | 2021-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |