http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113354825-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8c7c582c58ebb902c3111171ec32c641 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-285 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F7-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G83-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-226 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G83-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-28 |
filingDate | 2020-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78decf5dee4c8ee54005eb007809bd6a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_674758a960ffde9c7da27d799927f5b4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f87ff6efc6a76dd9802654db8c303c2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a12afd1947a9c990281cea8e8ffd26c4 |
publicationDate | 2021-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-113354825-A |
titleOfInvention | Zirconium-based metal-organic framework material UiO-66(Zr) and its rapid preparation method and application at room temperature |
abstract | The invention relates to a zirconium-based metal-organic framework material UiO-66(Zr) and a rapid preparation method and application thereof at room temperature. The preparation method includes: (1) after uniformly mixing a zirconium source and an organic ligand, placing it in methanol and stirring at room temperature , after centrifugation, the supernatant was discarded to obtain a transparent gel state intermediate product; (2) the intermediate product was heated and dried to obtain UiO-66(Zr). Compared with the prior art, the present invention does not involve the use of traditional solvothermal methods such as N,N-dimethylformamide and other toxic organic solvents, and UiO-66(Zr) can be synthesized by stirring and drying at room temperature in methanol. , the conditions are mild, the yield is high, the synthesis time is greatly shortened, and the product purity is extremely high, the step of product activation can be omitted, and the large-scale synthesis of this type of metal-organic framework material is very possible; the adsorption performance of fluoride ions in water is good , which can be applied to the adsorption treatment of fluorine-containing wastewater. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115671641-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115671641-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114773864-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114149593-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114149593-A |
priorityDate | 2020-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 59.