http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113353981-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c42baed8f638fbf4f93bcbeee153962b |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-36 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G31-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G31-00 |
filingDate | 2021-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9cc11e26ce3911277d748682f0d6e90a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc3b68f27aa99aca926a70c53db37992 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eb54744e1b8ea56cba769273225d4029 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_baafbf66cd44ddf9539ecf8f5d88be3a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_835283d0a126c4067a70a78a15ed5b81 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0d846332c4061c8989056909af86989 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d29b95e634538c461703a4780134b75d |
publicationDate | 2021-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-113353981-A |
titleOfInvention | A kind of preparation method of Cu3(VO4)2 irregular nanorods |
abstract | A method for preparing Cu 3 (VO 4 ) 2 irregular nanorods, wherein polypyrrole-coated cuprous oxide nanowires are used as templates and copper sources are dispersed in deionized water to obtain a suspension A; the suspension A is added with metavanadium Suspension B is obtained from ammonium acid powder; after the suspension B is sealed with plastic wrap, the product is separated after continuous stirring reaction at 25-100 ° C for 6-48 hours, and the separated product is washed with deionized water and absolute ethanol, and then Drying; laying the dried product on a porcelain boat, calcining the porcelain boat at 350-550° C. and cooling to room temperature to obtain Cu 3 (VO 4 ) 2 irregular nanorods. The invention uses cuprous oxide nanowires as templates, and through the process of in-situ crystallization, without changing the shape of the precursor template, the nanowires are converted into irregular nanorods composed of nanoparticles in an end-to-end manner ; Due to the isolation effect of the polypyrrole coating during the synthesis process, the obtained product can maintain the morphology of the irregular nanorods assembled by the particles. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114335578-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114335578-B |
priorityDate | 2021-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 43.