http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113214546-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_80c9b7fa466b9b47531c19e0b2124268 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2423-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2409-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2307-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2475-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0085 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-28 |
filingDate | 2021-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_104e9bbba49fc707917b6e16648c0fb8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93450db89e3942d4fc82e2cf235a7568 |
publicationDate | 2021-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-113214546-A |
titleOfInvention | A new type of thermal insulation and flame retardant rubber material |
abstract | The application discloses a novel thermal insulation and flame-retardant rubber material, comprising the following raw materials in parts by weight: 40-45 parts of natural rubber, 20-25 parts of polyurethane rubber, 30-35 parts of nitrile rubber, and 30- parts of chlorinated polyethylene 35 parts, 10-15 parts of rock wool fiber, 10-20 parts of graphite powder, 2-4 parts of foaming agent, 2-5 parts of plasticizer, 2-3 parts of vulcanizing agent, 4-7 parts of antioxidant, stabilizer 2-5 parts and 2-5 parts of curing agent; the processing temperature of the natural rubber, the polyurethane rubber, the nitrile rubber, the chlorinated polyethylene, the rock wool fiber and the graphite powder The temperature is 250-300°C, and the processing time is 40-50min. This application uses natural rubber, polyurethane rubber, and nitrile rubber as the main materials, so that it has excellent thermal insulation and corrosion resistance, and at the same time adds chlorinated polyethylene and rock wool fibers, so that the rubber material has good weather resistance. properties, chemical resistance, aging resistance, oil resistance, flame retardancy and coloring properties, enhance the environmental adaptation effect of rubber products. |