Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e344a64163315584afab21a745aae7b4 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-221 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-18 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5425 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-54 |
filingDate |
2021-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_74051ba2145121bf093b1a8ef79557cb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_28dd1a3785e850fb74f135b510b3706e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c8017a7c0a1e752ed89856758867d625 |
publicationDate |
2021-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-113185813-A |
titleOfInvention |
Method for preparing rigid-strength pipe by utilizing recovered hybrid PET containing PE and PA6 |
abstract |
The invention provides a method for preparing a rigid strength pipe by utilizing recovered hybrid PET containing PE and PA6, which is characterized in that the components are uniformly dispersed by regulating and controlling the distribution ratio of the components in the hybrid material and improving the selection aspect of a toughening agent SBR, the physical cross-linking points are increased by chain extension reaction, and the strength and the rigidity of the material are increased. The rigid strength pipe prepared by the invention has high performance, good toughness and wide application range. |