http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113150411-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2296 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-328 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2241 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2213 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-3009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-06 |
filingDate | 2021-05-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-113150411-B |
titleOfInvention | High-temperature and high-pressure resistant rubber pipe middle rubber and inner rubber comprehensive accelerator and preparation method thereof |
abstract | The invention relates to the technical field of rubber product processing aids, in particular to a high-temperature and high-pressure resistant rubber pipe middle rubber and inner rubber comprehensive accelerator and a preparation method thereof; the composite material comprises the following raw materials in parts by weight: 20-26 parts of mixed rubber, 0.8-1.2 parts of reinforcing agent, 1.5-2.0 parts of nano filler, 2.5-3.6 parts of performance reinforcing agent, 1.0-1.5 parts of nano molybdenum disulfide, 10-15 parts of zinc diphosphate, 12-20 parts of sulfonamide accelerator, 2-8 parts of thiazole accelerator, 5-10 parts of N-cyclohexyl thiophthalimide, 12-20 parts of 4, 4' -dithiodimorpholine, 3-10 parts of anti-blowout agent, 1-3 parts of dispersing agent and 25-35 parts of insoluble sulfur; the comprehensive accelerator prepared by the invention is used as a raw material for preparing the rubber tube, so that the prepared rubber tube not only has good ultraviolet resistance, ageing resistance and yellowing resistance; also has good antibacterial, anti-mildew, mechanical properties and high temperature, oil and high pressure resistance. |