http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112979991-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2387-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K2800-43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K2800-412 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2467-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2491-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2429-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G81-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K8-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K8-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K8-85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K8-922 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K8-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61Q19-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L91-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61Q19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G81-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L87-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-84 |
filingDate | 2021-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112979991-B |
titleOfInvention | A simple preparation method of environment-friendly structural color emulsion |
abstract | The invention relates to a simple preparation method of an environment-friendly structural color emulsion. Through the preparation of block polymer brushes, the preparation of polymer emulsion droplets and the preparation of structural color emulsion; the polymer is dissolved in an organic solvent, and through emulsification between the organic solution and the aqueous solution, when the organic solvent is completely volatilized, the The structural color emulsion has convenient preparation steps and avoids the tedious and complicated process of preparing environmentally friendly structural colors using cellulose as a template. The resulting structural color emulsion can be freely changed by changing the molecular weight or degree of polymerization of raw monomers and experimental conditions such as surfactant PVA concentration, organic solvent volatilization time, volatilization temperature and humidity, polymer concentration, vegetable oil content and other factors. The reflection wavelength of the droplet can be adjusted arbitrarily within the range of 320nm to 800nm. Structural color emulsions use environmentally friendly materials as raw materials, which have far-reaching significance for the development of green and sustainable pigments, and have potential applications in the production fields such as cosmetics. |
priorityDate | 2021-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |