http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112961451-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a24926fa9d6c9c67122c2afc5bbd1a0b |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2224 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2429-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2329-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-57 |
filingDate | 2021-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f830c6c85dd4dc9d41d93b79436ee856 |
publicationDate | 2021-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112961451-A |
titleOfInvention | A kind of crosslinking modified blown PVA high temperature water soluble film and preparation method thereof |
abstract | The invention relates to the field of degradable materials, and discloses a cross-linked modified blown PVA high-temperature water-soluble film. The blow-molded PVA high-temperature water-soluble film includes: PVA, a plasticizer, a thermal decomposition inhibitor, and an anti-thermal oxygen aging. agent, lubricant and anti-hydrolysis agent; relative to 100 parts by weight of PVA, the content of the crosslinking agent is 0.3-1 parts by weight, the content of the plasticizer is 5-50 parts by weight, the thermal decomposition inhibitor The content of the agent is 1-10 parts by weight, the content of the anti-thermal oxidative aging agent is 0.5-5 parts by weight, the content of the lubricant is 0.1-5 parts by weight, and the content of the anti-hydrolysis agent is 0.1-1 parts by weight. The blow-molded PVA high-temperature water-soluble film provided by the invention can realize continuous granulation and blow-molded film-forming of the high-temperature water-soluble PVA. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115636970-A |
priorityDate | 2020-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 95.