http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112961406-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-323 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-32 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 |
filingDate | 2021-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112961406-B |
titleOfInvention | A kind of confined polymerization flame retardant and preparation method thereof |
abstract | The invention relates to the technical field of flame retardants, in particular to a confined polymerization flame retardant and a preparation method and application thereof. In the confined polymerization flame retardant, ammonium polyphosphate is confined in the halloysite cavity. In the confined polymerization flame retardant, the average diameter of the halloysite is less than or equal to 5 nm. The specific surface area of the confined polymerization flame retardant is less than or equal to 3.0 m 2 /g. Advantages of the present invention: (1) Overcoming the problem of poor compatibility between ammonium polyphosphate and polymer materials, and adding to the material as a flame retardant leads to a significant reduction in the mechanical properties of the material. (2) The flame retardant properties and mechanical properties of the material can be significantly improved at the same time. (3) Effectively improve the defect of high water solubility of ammonium polyphosphate. (4) The preparation method is simple, low in cost, easy to operate and popularize. |
priorityDate | 2021-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |