http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112939584-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_94efc5c0bbb98a398a4c03111940f9a9 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6567 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3206 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3418 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C4-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C4-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27D1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C4-134 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C4-134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C4-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27D1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C4-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-10 |
filingDate | 2021-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a1118c78681a9fb337fa3cf4dd56b937 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff6e55318fdef110688d64efff8d68ab |
publicationDate | 2021-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112939584-A |
titleOfInvention | A ceramic/metal composite furnace tube and its preparation method and application |
abstract | The invention provides a ceramic/metal composite furnace tube and a preparation method and application thereof, belonging to the technical field of furnace tubes. The ceramic/metal composite furnace provided by the invention relies on the large size of the metal furnace tube, and by loading a layer of ceramic layer on the outer surface of the metal furnace tube, the disadvantage that the furnace tube cannot be made larger and longer due to the ceramic material as a whole is avoided. The corrosion of the metal furnace tube by corrosive materials ensures the large size of the metal furnace tube. In addition, the material composition of the ceramic layer designed in the present invention makes the ceramic layer and the metal furnace tube made of stainless steel have the same expansion coefficient, which avoids the situation of cracking due to the different expansion coefficients of the matrix and the load layer, and expands the metal furnace tube. Scope of application. The preparation method of the ceramic/metal composite furnace tube provided by the invention enables the ceramic/metal composite furnace tube to have excellent strength. |
priorityDate | 2021-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |