Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_764bbcdeffecda3dbf6027c594dadac3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_74d751f64357d2ca0a14106168770e21 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E02D17-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E02D3-126 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C12N1-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E02B3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E02D3-12 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12R1-07 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12N1-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E02D17-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E02B3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E02D3-12 |
filingDate |
2020-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df8c08791efdb7a84831a7d8d6a09be0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8864f7d3837fc47f435532661f300be2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6611bd060481b2a3a64f7eb21feeee84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b763833b2e4c2912f05a223d81e4cea8 |
publicationDate |
2021-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-112813960-A |
titleOfInvention |
A method for improving expansive soil reinforced with microbial composite fibers |
abstract |
Disclosed is a method for improving expansive soil reinforced with microbial composite fibers, comprising: culturing microbial strains in a fermenter according to optimal culture conditions to form microbial bacterial liquid; Mix the mixed calcium solution and stir in a low-speed mixer to form a microbial slurry; add reinforcing materials and mix with the expansive soil to form a fiber-reinforced expansive soil; according to the 20% moisture content, the microbial slurry and the fiber-reinforced The expansive soil is mixed in batches at a weight ratio of 1:5 in a low-speed mixer and evenly stirred, and cured at room temperature to obtain an improved expansive soil. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113417295-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113417295-B |
priorityDate |
2020-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |