http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112794642-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B37-012 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B37-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B37-01211 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J43-246 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C15-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B37-012 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B37-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J43-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C15-00 |
filingDate | 2021-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2023-01-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2023-01-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112794642-B |
titleOfInvention | Borosilicate matrix glass material for microchannel plate and preparation method thereof |
abstract | The invention discloses a borosilicate matrix glass material for a microchannel plate and a preparation method thereof. The borosilicate matrix glass material for a microchannel plate includes a core glass and a skin glass, and the components of the skin glass include SiO 2 , B 2 O 3 6 , Al 2 O 3 , Na 2 O, K 2 O and CaO; the composition of the core glass includes SiO 2 , B 2 O 3 , BaCO 3 , La 2 O 3 , Al 2 O3 and ZnO. The invention has a reasonable formula, replaces lead and other hazardous chemicals, and reduces environmental pollution. The core glass can be dissolved in high-speed acid without leaving residues. The skin glass has good corrosion resistance and mechanical properties, and has the advantages of preventing MCP from deforming and having a uniform structure. The invention has the advantages of good performance and pore diameter precision, and the raw materials of the invention are easy to obtain, the cost is not high, it is easy to melt and shape, and the production and preparation efficiency is high. |
priorityDate | 2021-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 34.