http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112723491-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_47abb4a6aebec50d0898d51055043601 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2001-46133 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2001-46161 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-46109 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-461 |
filingDate | 2020-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb520c3005c9b34aca6299d9d27affb8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_32d517a95bf46a03cc99e0f4ba38beef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8880b20ded606f1134d49c68207a2171 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d8b66fe42bae1a2008bc8be72461262d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_acb3f904a163fb9f1839d5910b4a5bf1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_69cccd6895db599967032291410c3e0c |
publicationDate | 2021-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112723491-A |
titleOfInvention | Capacitive desalination electrode material and preparation method thereof, capacitive desalination electrode and preparation method thereof |
abstract | The invention relates to a capacitive desalination electrode material and a preparation method thereof, a capacitive desalination electrode and a preparation method thereof, belonging to the technical field of electric desalination electrodes, and a preparation method of a capacitive desalination electrode material, comprising: combining zinc nitrate hexahydrate and triethylene Diamine is dissolved in the first N,N dimethylformamide solution to obtain a first mixed solution; terephthalic acid is dissolved in the second N,N dimethylformamide solution to obtain a second mixed solution; The first mixed solution and the second mixed solution are mixed, refluxed and stirred in an oil bath, dried, cooled, washed once, and dried once to obtain a dual-ligand metal-organic framework Zn-MOF; under an inert atmosphere, Carbonizing the Zn-MOF, placing the carbonized Zn-MOF in an acid solution to react, and after secondary washing and secondary drying, a capacitive desalination electrode material is obtained, and the capacitive desalination electrode material is a double ligand Zn-MOF-derived nitrogen-doped rod-like porous carbon materials. |