http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112646444-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-26 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-443 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-446 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-434 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 |
filingDate | 2020-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112646444-B |
titleOfInvention | Preparation method of mesoporous silica water-based ceramic slurry |
abstract | The invention relates to the technical field of lithium ion battery coating diaphragms, and discloses a preparation method of mesoporous silica aqueous ceramic slurry, which comprises the following steps: A. placing mesoporous silica nano particles under an acidic condition, chemically modifying the mesoporous silica nano particles by using a silane coupling agent to prepare an ethylene mesoporous inorganic particle intermediate, and reserving the intermediate for later use; B. and B, adding the vinylated mesoporous inorganic particle intermediate prepared in the step A into a mixed system consisting of active monomers of isooctyl acrylate, methyl methacrylate, acrylonitrile, 2-ethyl hexyl acrylate, acrylamide, an emulsifier and an initiator, polymerizing by an emulsion polymerization method to prepare a water-based block copolymer, and obtaining the mesoporous silicon oxide water-based ceramic slurry. The invention solves the problem of poor heat resistance of the existing battery diaphragm. |
priorityDate | 2020-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 71.