http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112620610-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b4ea77aa0aee98305b2f734bd3c1984e
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5fe1f64aeb15511c31677dc69cf660d8
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B1-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22D19-00
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28B1-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D19-00
filingDate 2020-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_13c79651127c9f9113a41949c42de310
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4f8e12ccb7d09227b07030f2320f6631
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_55425f701c80b3760d8678e3f4d9f66f
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a5ab6bfd262da8f3a68d4fd7b1b45eca
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_641d903ec9ebb4069b5d2cfc327640d1
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_904f7d5d2288327598d02d154a45e3ea
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b204d808f92cb2e672c7648bd1eb925
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f2cfef2edd67e69f73f804253da4af64
publicationDate 2021-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-112620610-A
titleOfInvention Ceramic-metal composite formed part, preparation method thereof and wear-resistant part
abstract A ceramic-metal composite formed part, a preparation method thereof and a wear-resistant part belong to the technical field of composite materials. The preparation method of the ceramic-metal composite molded part comprises the following steps: and mixing and sintering the ceramic particles and the binder to form the ceramic preform. And under the condition that the ceramic preform keeps the residual heat after sintering, placing the ceramic preform in a casting mould for metal melt casting, and performing pressure composite molding after casting. Which can increase the interfacial bonding strength of metal and ceramic.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113683402-A
priorityDate 2020-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID449134064
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID84353
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID450183
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID539003
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID30265
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID395964
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID477032
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID12387
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID159387
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID1499

Total number of triples: 32.