http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112537798-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5923afb26d308a3193fd4ef69283b762 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G51-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 |
filingDate | 2020-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36626e9f1aa12ade19d17c67fb7d9064 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c4a79a8f9c170140e16b9473c133a44e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_96e3ec894c6a110ea6fc45f196c3d42f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98d73df0a5dc62fadde4c648ecd26b0a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8d2b8170da6210e60c1326056b080a57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_74328ae36ae9676f44999f6229b61ddb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c8e9464042119a0f153c0315c59f1de |
publicationDate | 2021-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112537798-A |
titleOfInvention | A kind of preparation method of zinc cobaltate nanowire |
abstract | The invention provides a method for preparing zinc cobaltate nanowires. Cobalt chloride hexahydrate, zinc chloride and nitrotriacetic acid are added to deionized water, and magnetic stirring is performed until they are completely dissolved; then isopropanol is added to form a mixed solution, The mixed solution is transferred to a polytetrafluoroethylene reactor for hydrothermal reaction, and after the reaction is completed, it is cooled to room temperature, and the zinc cobaltate precursor product is obtained by washing with water and ethanol, centrifuging, and then drying in a vacuum drying box; The resulting zinc cobalt oxide product is heated in a muffle furnace to obtain mesoporous zinc cobalt oxide nanowires. The preparation method provided by the invention is rich in raw material resources, low in price, stable in production, high in yield, environmentally friendly and convenient for industrial production. The as-prepared zinc cobaltate nanowires have a porous hollow structure, which can effectively accommodate volume expansion and shorten the transfer distance of Li + and electrolyte, and can also accommodate huge volume changes during Li + insertion/extraction. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114400319-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114394627-A |
priorityDate | 2020-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 48.