http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112226805-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3481daaa40c1ddded0de2124c9344f70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2e40e7dbbee6b82bbd1a0d3356f00e55 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-50 |
filingDate | 2020-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43a96f3efdcf8d5c02f715fb37d3da71 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7438cbc8c3b956635c5b03f8a600fe5e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0e09815611c902820923e37350c5d782 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6208540e7aca244be59f55814441a056 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4818e0d4354c97b74fdb6aabb43714f6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a07d2079cb85fbe2de759ac155cb035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_96ef4a8f5c3e29bc54569d1c40b8066d |
publicationDate | 2021-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112226805-A |
titleOfInvention | A kind of preparation method of electrodeposited cobalt-based composite coating |
abstract | A preparation method of an electrodeposited cobalt-based composite coating layer belongs to the technical field of surface protection. The method includes the following steps: (1) preparing a composite plating solution, which is prepared from cobalt sulfate, cobalt chloride, boric acid, phosphoric acid, surfactant and water. (2) Add the pretreated ceramic powder to the composite plating solution and stir to make the powder evenly dispersed in the plating solution. (3) Composite electrodeposition is carried out by using pulse current and two-electrode parallel device, the cleaned cobalt plate is used as the anode, the workpiece to be plated is the cathode, and a cobalt-based composite coating is formed on the surface of the workpiece to be plated. (4) The workpiece on which the cobalt-based composite coating is formed is heat-treated. The invention adopts technical means such as using pulse power supply to replace DC power supply, adjusting current density, heat treatment of coating layer, chemical pretreatment of powder particles, etc., so as to significantly improve the bonding strength of powder particles and metal matrix, improve the uniformity of the coating layer, and reduce the roughness of the coating layer. degree, and enhance the coating performance. |