http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112174210-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2c1518dc9cc02a9f9b927853433b08f1 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G41-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G41-00 |
filingDate | 2020-09-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c5d1969bdc146bcf663da74a44d6b117 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2050a231fd43aae1807b059c45974b3e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_813ae7703d3d66eedb8a1cdf38868270 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3533c9b531f0981f22bfdf06a4eaafa |
publicationDate | 2021-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112174210-A |
titleOfInvention | Preparation method of water-based dispersion-free nano cesium tungsten oxide coating |
abstract | The invention relates to the technical field of nanomaterials, in particular to a preparation method of an aqueous dispersion-free nanometer cesium tungsten oxide coating. The preparation method of the water-based dispersion-free nano cesium tungsten oxide coating is to weigh cesium salt and tungsten salt, add a chelating agent and water, heat up to 150-160 ° C and react for 5-6 h; and then under ultrasonic conditions, heat up React at 230-260°C for 3-4h to obtain a dispersion of cesium tungsten oxide; then cool to 50-80°C, add an aqueous dispersant and a defoamer, heat up to 160-180°C for activation reaction for 5-6h, and obtain Activated nano-cesium tungsten oxide sol; finally concentrated to a solid content of 45-50%, spray-dried to obtain a water-based dispersion-free nano-cesium tungsten oxide coating. The preparation method of the water-based dispersion-free nano cesium tungsten oxide coating body of the present invention has the advantages of simple process, short preparation period, cost saving, no need for secondary grinding, safe and convenient storage and transportation. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109641449-A |
priorityDate | 2020-09-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 48.