http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112143185-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-0806 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-1345 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2227 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5425 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2467-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-226 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-92 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5425 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-22 |
filingDate | 2020-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-112143185-B |
titleOfInvention | A kind of antibacterial and deodorant polyester masterbatch and its manufacture method and polyester fiber |
abstract | The invention discloses an antibacterial and deodorizing polyester master batch, a manufacturing method thereof and polyester fiber. The polyester masterbatch contains 50-80 parts of polyester, 5-10 parts of water-soluble polyester, 5-20 parts of silver-loaded porous material, 1-5 parts of dispersant, 0.5-1 part of antioxidant, and 0.5-1 part of coupling agent 1.5 parts; the viscosity ratio of polyester to water-soluble polyester is 5-20:1; preparation method: first use a high-temperature kneader to melt and knead polyester, silver-loaded porous material, dispersant, antioxidant, and coupling agent to obtain polyester Melt; then add water-soluble polyester to polyester melt to extrude and granulate, and use the strong shearing action of the extruder to mix the water-soluble polyester and polyester melt evenly and then extrude. The polyester fiber made of the polyester masterbatch, in which the water-soluble polyester flows to the outer layer of the fiber and can be eluted by hot water, makes the silver-loaded porous material have a microporous structure that communicates with the outside world, deodorizing and antibacterial substances It is easier to be exposed to bacterial odor, and the antibacterial and deodorizing functions are improved. |
priorityDate | 2020-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |