http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111960701-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G49-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B03C1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B12-005 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03C1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G49-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B12-00 |
filingDate | 2020-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-111960701-B |
titleOfInvention | Full-scale utilization method for reducing, roasting, separating and recovering iron and silicon-aluminum synchronous activated red mud |
abstract | The invention discloses a full-scale utilization method of red mud for synchronous activation of reduction roasting separation recovery iron and silicon-aluminum, belonging to the field of solid waste treatment and resource utilization. Drying the red mud, grinding the dried red mud into powder, adding a carbon-based reducing agent, reducing and roasting, wherein ferric oxide in the red mud is reduced into ferroferric oxide, ferrous oxide and an iron simple substance, and meanwhile, silicon-aluminum elements in the red mud are activated; mixing the reduction roasting intermediate product with water, performing magnetic separation by using a magnetic separator to obtain an iron concentrate product, and filtering the magnetic separation suspension to obtain magnetic separation residues; mixing the magnetic separation residue with fly ash, adding sodium hydroxide, potassium hydroxide or water glass, and adding water to obtain a clean slurry; and pouring the clean slurry into a mold, heating and curing under a sealed condition, taking out the mold, demolding, and performing standard curing to obtain the geopolymer. The invention realizes the resource recovery and full-scale utilization of the red mud, and has the characteristics of high utilization rate of solid waste, good mechanical property of products and low production cost. |