http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111725556-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b63b312996de4a4ff40c2dc82b289624
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0566
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-44
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-42
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-4235
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-583
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-5825
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-583
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-58
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0566
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-44
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-42
filingDate 2020-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5698e9bda78b8936390e39932f81aa90
publicationDate 2020-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-111725556-A
titleOfInvention A kind of storage method of lithium iron phosphate battery
abstract The invention provides a storage method of a lithium iron phosphate battery, wherein the positive electrode active material of the battery is LiFe 1-x Nb x PO 4 , wherein x is 0.02-0.04, and the negative electrode active material of the battery is a graphite material; The electrolyte of the battery contains 1.5-1.8 volume % of butyl methanesulfonate and 0.5-1 volume % of bromobutyrolactone; the storage method includes: constant current discharge to discharge cut-off voltage, and then at 1C The above current is charged to the first predetermined voltage with constant current, the battery temperature is adjusted to above 50 degrees Celsius, left for a predetermined time, the open circuit voltage of the battery is measured, and it is judged whether the first predetermined voltage-the open circuit voltage is greater than or equal to a predetermined value, according to the judgment result The subsequent treatment process is determined; the lithium iron phosphate battery obtained by the storage method of the present invention has low storage capacity attenuation and can maintain good cycle retention performance.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112909337-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112234270-A
priorityDate 2020-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID415796713
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID95463
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID414878929
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID449015670
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID15953
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23688915
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID15320824
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID447735963

Total number of triples: 33.