http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111647960-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D10-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-94 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-0885 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D10-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-94 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10 |
filingDate | 2020-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-111647960-B |
titleOfInvention | Manufacturing method of loss-reducing and resistance-reducing wire for marine ranching |
abstract | The invention provides a method for manufacturing loss-reducing and resistance-reducing yarns for marine ranches, which comprises three procedures of raw material compounding, melt spinning, stretching and heat setting, wherein POK granules, zinc stearate, silicone powder, an antioxidant and white oil are used as raw materials, a POK composite material is obtained firstly, and then the POK composite material is extruded by a double-screw extruder, subjected to spinning, drafting, heat setting and yarn splitting, so that POK fibers are obtained. The POK fiber prepared by the method for preparing the loss-reducing and resistance-reducing yarn for the marine ranching has the excellent performances of smooth surface, high strength, wear resistance and the like. The preparation method is simple, the preparation process is low-carbon and environment-friendly, and the production cost can be obviously reduced. |