http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111635737-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K3-149 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 |
filingDate | 2020-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-111635737-B |
titleOfInvention | Efficient nano anti-slip agent with self-cleaning function for floor tiles and preparation method thereof |
abstract | The invention discloses a high-efficiency nano anti-slip agent for floor tiles with a self-cleaning function and a preparation method thereof, wherein the high-efficiency nano anti-slip agent for floor tiles with the self-cleaning function comprises the following components in parts by mass: 20-40% of fruit acid, 2-5% of ammonium bifluoride, 2-10% of ammonium fluoride, 10-15% of special antifouling emulsion, 8-25% of citric acid, 3-8% of alcohol, 4-10% of plant powder, 0.1-1% of dispersion stabilizer, 0.5-1% of defoaming agent, 0.5-0.75% of bactericide, 10-20% of glycerinated rosin, 1-4% of oxalic acid, 10-15% of composite ionic surfactant, 4-7% of hydrophilic chain extender, 0.2-6% of air entraining agent, 0.5-1% of corrosion inhibitor and the balance of water, wherein the surface friction coefficient before and after use of the floor tile can be increased from 0.2-0.6 to 0.9-2.3, and the floor tile has higher hardness and longer service life, can form a hydrophobic layer on the surface of the floor tile to prevent the permeation of various stains, the self-cleaning effect is achieved. |
priorityDate | 2020-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |