Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L95-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L95-00 |
filingDate | 2020-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-111560157-B |
titleOfInvention | An instant low-isolation high-viscosity high-elasticity modifier and its preparation method and application |
abstract | The invention discloses an instant modifier with low segregation degree, high viscosity and high elasticity, which is mainly prepared from the following components in parts by weight: 50-80 parts of TPEE, 12.5-30 parts of PTW, and 1-2.5 parts of monoglyceride , 5-19 parts of PBAT, the present invention also discloses a preparation method and application of an instant low-isolation, high-viscosity and high-elasticity modifier. The TPEE selected in the present invention has good viscoelasticity, and the dispersibility of PBAT and PTW is good. In addition, monoglyceride is used as a lubricant, and various components cooperate with each other, which is fully compatible with asphalt, and gives full play to the performance of each component. The material forms an instant modifier with low segregation, high viscosity and high elasticity. The asphalt modifier is added to the asphalt to be fully mixed with the asphalt and has better dispersibility, which not only makes the modified asphalt have good properties. Viscous and elastic, can also improve road pan-axle, rutting. |
priorityDate | 2020-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |