http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111540970-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7518988c98e8bdaec07bcbd37a6dd68c
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0025
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-44
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-4235
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-5825
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0567
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-58
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-44
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-42
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0567
filingDate 2020-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2edb67df14420a68eebecfdeeb96a2ef
publicationDate 2020-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-111540970-A
titleOfInvention A kind of storage and activation method of lithium iron phosphate battery
abstract The invention provides a storage and activation method of a lithium iron phosphate battery, wherein the positive active material of the lithium iron phosphate battery comprises lithium iron phosphate or modified lithium iron phosphate accounting for more than 85% of the total mass of the active material; the battery The electrolyte includes dimethyl sulfoxide and butyl methanesulfonate as additives; the first predetermined voltage is lower than the second predetermined voltage, and the first predetermined voltage is 3.35-3.44V; the second predetermined voltage The voltage is 3.40‑3.45V; the battery is stored for a period of time, the battery is pulse charged to the second predetermined voltage, then discharged with constant current to the discharge cut-off voltage, then charged with constant current to the second predetermined voltage, and charged with the second predetermined voltage and constant voltage, Until the current is lower than the cut-off current, and then constant current charge to the charge cut-off voltage. The lithium iron phosphate battery subjected to the present method can be stored for a long time and can substantially maintain the capacity before storage after storage.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112909337-A
priorityDate 2020-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419538066
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID447735963
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID15953
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID414878929
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID15320824
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID679
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID449015670
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23688915

Total number of triples: 28.