http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111518553-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01K11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N21-6428 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y20-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-65 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01K11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N21-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y20-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-03 |
filingDate | 2019-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-111518553-B |
titleOfInvention | Preparation method and application of water-phase room-temperature phosphorescent carbon dot material |
abstract | The invention discloses a preparation method and application of a water-phase room-temperature phosphorescent carbon dot material, and belongs to the field of manufacturing of functional luminescent carbon materials. According to the invention, a carbon source, a molten salt matrix, an alkaline earth metal salt and a hydrogen phosphate are mixed and carbonized, after the carbonization is finished, the temperature is cooled to room temperature, and the molten salt matrix of the prepared material is washed and removed, so that the room-temperature phosphorescent carbon dot material with water dispersion property is obtained. The method effectively solves the problems that the existing carbon dot phosphorescent material cannot be applied to a water phase, has short service life and complex preparation method, and can be used for simply manufacturing a large batch of room temperature phosphorescent materials which can be applied to the water phase. |