http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111468096-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d40285e27f4ed83b8728b0d477404958
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W10-37
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-308
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-026
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-002
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-30
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-10
filingDate 2020-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ce2a714f6df525acd7ffb09555576a9
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4e10be0ecbe1c9ce058206daee076479
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_38ed2ba598d23e34c9f7eab9c51cac1f
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1b4ace6bbcc04f902d667a628a7fffd
publicationDate 2020-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-111468096-A
titleOfInvention A kind of Zn2TiO4/TiO2 composite material and its preparation method and application
abstract The invention relates to a preparation method of Zn 2 TiO 4 /TiO 2 composite material . 3 to 4; S2, place the mixed solution obtained in step S1 under constant temperature stirring under a preset temperature environment, and dropwise add CO(NH 2 ) 2 solution to adjust the pH of the mixed solution to 5 to 7; S3, obtain step S2 The mixed solution is subjected to a hydrothermal reaction, and the product of the hydrothermal reaction is calcined. The invention adopts two steps to adjust the pH of the solution. The first step can effectively neutralize the strong acid H 2 SO 4 mixed with the reagent ZnSO 4 and TiOSO 4 ; 2. Uniform and slow decomposition, which can provide evenly precipitated hydroxide ions for the preparation of composite materials, and effectively ensure the uniform composite of products.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114558561-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112108140-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111905748-A
priorityDate 2020-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID407275646
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14798
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID8534
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419476681
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID409060395
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID4139
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23673835
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419572355

Total number of triples: 38.