abstract |
The present invention relates to a composition for producing thermoplastic molding compounds, wherein the composition comprises or consists of the following components: A) 50-90% by weight of a compound having CH2Cl2 as solvent at 25 °C and 0.5 g Aromatic polycarbonate or polyester carbonate having a relative solution viscosity of at least 1.285 measured at a concentration of 100 ml, B) 1-10% by weight of rubber-modified graft polymer, C) 2.5-10% by weight Boron nitride, D) 4-20% by weight of talc, E) 2-20% by weight of a phosphorus-containing flame retardant, F) 0-20% by weight of other additives, and a process for producing thermoplastic molding compounds, the molding compounds themselves , the use of molding compounds for the preparation of moldings, and the moldings themselves. |