http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111393117-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00767 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-27 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B09B3-21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-006 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-27 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-08 |
filingDate | 2020-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-111393117-B |
titleOfInvention | Water-containing undisturbed shield muck baking-free building material and preparation method thereof |
abstract | The invention relates to a water-containing undisturbed shield muck non-fired building material and a preparation method thereof. The preparation method is characterized in that the baking-free building material is composed of the following raw materials in parts by weight: 1-80 parts of water-containing undisturbed shield muck, 1-30 parts of active waste residue, 0.1-5 parts of sodium hydroxide, 0.1-10 parts of sodium silicate and 1-20 parts of water, and comprises the following steps: weighing active waste residues, sodium silicate, water-containing undisturbed shield muck and water, mixing and crushing until the content of particles with the particle size of 4.75mm or more than 5mm in the water-containing undisturbed shield muck is not more than 10%, and obtaining a mixture I; adding sodium hydroxide into the mixture I to obtain a mixture II; and pouring the mixture II into a mold to obtain the water-containing undisturbed shield muck non-fired building material. The method saves the intermediate dehydration and screening processes and links, and greatly reduces the production cost. The invention also discloses the water-containing undisturbed shield muck baking-free building material prepared by the method. |