http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111348871-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_66e14891ed87b705b60e44596c647cfd
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00017
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2201-50
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2201-20
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-021
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-144
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-04
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02
filingDate 2018-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d54c9f4dc52ac86f1527f85f97d804f3
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dc35a2161063ec1c092807d507f5032
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f60c3b6157d52df241ac71406b8e79b8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51cbafc94d690346a58527ef9684d1f9
publicationDate 2020-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-111348871-A
titleOfInvention A kind of high titanium slag sand active powder concrete and preparation method thereof
abstract The invention provides a high titanium slag sand active powder concrete and a preparation method thereof. The preparation method comprises: drying, crushing and grading high titanium slag to obtain graded high titanium slag sand; Fly ash, silica fume and steel fibers are mixed uniformly, then water and water reducing agent are added to obtain a slurry; the graded high titanium slag sand is mixed with the slurry, molded and cured to obtain active powder concrete . The active powder concrete is calculated in parts by mass, including 55 to 65 parts of high titanium slag sand, 15 to 24 parts of cement, 5 to 8 parts of fly ash, 2.5 to 4 parts of silica fume, and 2 to 5.5 parts of steel fiber. parts, 4.5 to 8.5 parts of water, and 0.5 to 1.0 parts of water reducing agent. The products prepared by the method of the invention have high compressive strength and flexural strength, can be used for preparing underground railway passages and sleepers, and can also be applied to engineering structures such as sponge city construction, underground pipelines and prefabricated pipe galleries, and are widely used.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112830726-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111906923-A
priorityDate 2018-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559477
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24261
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707758
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23963
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635

Total number of triples: 30.