http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111164165-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-03 |
filingDate | 2018-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-111164165-B |
titleOfInvention | Powder coating composition and method for forming coating film |
abstract | The powder coating composition of the present disclosure has an excellent appearance, can form a smooth coating film, can form a coating film having excellent impact resistance and excellent scratch resistance. A powder coating composition comprising an acrylic resin (A) and a polyester resin (B) as coating film forming resins, wherein the acrylic resin (A) has an epoxy group, has a solubility parameter SP (A) of 9.0 to 12.0 inclusive, has an average molecular weight of 500 to 4,000 inclusive, and has an epoxy equivalent of 200g/eq to 500g/eq inclusive in the acrylic resin (A), the polyester resin (B) has a carboxyl group, and has a solubility parameter SP (B) of 9.0 to 11.0 inclusive, and the absolute value | SP (A) -SP (B) | obtained by subtracting the solubility parameter SP (B) from the solubility parameter SP (SP A) is 0 to 2 inclusive. |