http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111051061-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-124 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-312 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-255 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-042 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-401 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2018-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_13fc78548e935f39eba2b6f977f08557 |
publicationDate | 2020-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-111051061-A |
titleOfInvention | Release film and laminate |
abstract | A release film comprising a cross-linked resin layer on at least one side of a polyester film stretched at least in a uniaxial direction, and a release film having a release layer laminated on the cross-linked resin layer, The cross-linked resin layer is formed of a cross-linked resin composition containing a cross-linking agent (C) and an ionic polymer (A) having a cationic group, and the release layer is formed of a release agent composition. The molding agent composition contains a first polydimethylsiloxane having a weight average molecular weight of 500 to 50,000 and having at least one alkenyl group in one molecule, and a weight average molecular weight of 120 to 20,000 and having at least one hydrogenated group in one molecule. The second polydimethylsiloxane of the silyl group has a peeling force of 4 g/25 mm or less when measured by the following method. <Measurement of peeling force> The mold release layer of the mold release film and the adhesive tape (manufactured by Nitto Denko Co., Ltd., "No. 502", acrylic pressure-sensitive adhesive) were bonded together, and the film was stretched at a tensile speed of 300 mm/min. 180° peel test under conditions. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115322426-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114350260-A |
priorityDate | 2017-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 243.