Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_85f309a0eec998875e57a9cf79579b4c |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F283-124 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 |
filingDate |
2019-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f3a9722ac6d586c9c1d33dc4a26ccbc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_11d27ebf8d32a58c567961829a1e9ede http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3884c92648ea4241f197ca6ccb17f747 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61fb9da30118728ffb37145812c66d79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31ec07d6c229ddc70e042044d1566b36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6eca38960880b70383656b0a6b2ee6f2 |
publicationDate |
2020-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-111040504-A |
titleOfInvention |
A kind of defoamer for solvent-based paint and preparation method thereof |
abstract |
The invention discloses a defoaming agent for solvent-based coatings and a preparation method thereof, comprising the following raw materials in terms of weight percentage: 5-40% of modified acrylate; 3-20% of long-chain alkyl silane; 0.5% of white carbon black ~5%; 0.1~2% of catalyst; 0.1~2% of crosslinking agent; 30~90% of solvent; 1~20% of auxiliary agent. Long time, and make the coating surface have better waterproof and anti-corrosion performance. |