http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111019520-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1687 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D161-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 |
filingDate | 2019-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-111019520-B |
titleOfInvention | Low-density flame-retardant wear-resistant long-acting anti-pollution flashover coating and preparation method thereof |
abstract | The invention discloses a low-density flame-retardant wear-resistant long-acting anti-pollution flashover coating and a preparation method thereof, wherein the coating comprises a component A and a component B; uniformly stirring basic silica gel, vinyl-terminated fluorosilicone oil, modified polyether ether ketone micro powder, methyl phenyl silicone oil, an antistatic agent and a platinum catalyst in a certain proportion in vacuum, removing bubbles, and filtering impurities to obtain a component A; uniformly stirring basic silica gel, vinyl-terminated fluorosilicone oil, modified polyether ether ketone micro powder, methyl phenyl silicone oil, a tackifier, a cross-linking agent and an inhibitor in a certain proportion in vacuum, removing bubbles, and filtering impurities to obtain a component B. The silicone rubber is constructed in a solvent-free dip-coating mode, the operation time is more than or equal to 24 hours at normal temperature, the silicone rubber is quickly vulcanized at high temperature, the density is low, the flame retardant property reaches FV-0 level, the wear resistance reaches 5 level, the good bonding of glass and a ceramic insulator can be realized, the prepared insulator has excellent performance, and the impact breakdown performance can reach 2.8 p.u.. |