http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110914348-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5f7f120efe096284c7389702c969cf3d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2309-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-026 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-228 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-228 |
filingDate | 2018-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82995fade8733716be6d2906902942fd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eeae7e071f6e6eebde2a8ba4dfbec1b6 |
publicationDate | 2020-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110914348-A |
titleOfInvention | Manufacturing method of foam rubber |
abstract | The present invention provides a method for producing foamed rubber, wherein foamed rubber is produced by foaming a polymer latex, and as the polymer latex, a polymer latex having a solid content concentration of 60.0% by weight or more and the polymer latex described above is used. The content ratio of the antifoaming agent to 100 parts by weight of the polymer is 0.001 to 1.0 parts by weight, and the viscosity at a temperature of 25°C when the solid content concentration is adjusted to 66.0% by weight is 370 cps or less. |