http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110900475-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B24D18-0072 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B24D11-001 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B24D11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B24D18-00 |
filingDate | 2019-12-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110900475-B |
titleOfInvention | Flexible coating abrasive cloth |
abstract | The invention discloses a flexible coating abrasive cloth which is prepared according to the following procedures: preparing a base material, singeing, alkali washing, water washing, high-temperature shaping, dipping, stretching, drying and shaping, sizing, sand planting, drying, glue compounding, drying, post-curing, kneading, detecting product performance, coiling and packaging, wherein: (1) dipping, namely putting the base material into dipping liquid to dip for 10-15min at 40-50 ℃, stretching, drying and shaping, drying the base material by a shaping machine, presetting at 110-120 ℃, and then shaping at 200-210 ℃; (3) electrostatic sand planting, wherein the abrasive is bonded on the surface of the primer of the base material through the electrostatic sand planting; the abrasive cloth has good grinding efficiency, anti-blocking effect and service life, improves efficiency, saves energy consumption and reduces cost. |