http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110857365-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1687 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D1-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D1-04 |
filingDate | 2018-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110857365-B |
titleOfInvention | Composite coating and preparation method and application thereof |
abstract | The invention discloses a composite coating and a preparation method and application thereof. Wherein, the composite coating comprises: 10 to 30 wt% of lithium silicate; 5 to 15 wt% of potassium silicate; 0.5-5 wt% of modified siloxane; 0.1 to 1 wt% of a wetting agent; and the balance water. The composite coating has better stability by optimally controlling the proportion of the lithium silicate and the lithium silicate. Furthermore, the coating formed by the composite coating has lasting and excellent easy-cleaning performance, wear resistance, acid resistance and alkali resistance, and is wide in application range. |