http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110804205-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8a49950b0d9bc27732fc556f3467824d
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-40
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-141
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G23-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B38-0054
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G9-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B38-0045
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F7-021
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-24
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-04
filingDate 2019-12-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9110bb7fefcafeedb32e5eb6b3f5f4dc
publicationDate 2020-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-110804205-A
titleOfInvention Water-soluble resin thermal insulation material with nanoporous structure and preparation method thereof
abstract The invention discloses a water-soluble resin thermal insulation material with a nanoporous structure and a preparation method thereof. The preparation method of the water-soluble resin heat-insulating material with nano-porous structure is to heat a preform with a water-soluble resin as a skeleton in which an appropriate amount of water is uniformly dispersed to vaporize the molten resin and maintain its shape; The volume is increased to achieve the desired porosity; and the water-soluble resin thermal insulation material with nanoporous polymer skeleton structure is obtained by cooling.
priorityDate 2019-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID7913
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID449603119
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID62705
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID19096565
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419587169
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451403919
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419546195
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID10541

Total number of triples: 34.