Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_eb83ef3cdd579390b2ae3a73ee8265f7 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J161-12 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J125-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J161-12 |
filingDate |
2019-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_60e46e1abe2df662a2bec5146ebf0fdc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c973f647e61575f093420326527b31fc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2408d7465cea36e74363927cb042df3 |
publicationDate |
2020-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-110791241-A |
titleOfInvention |
A kind of preparation method of resorcinol adhesive for tires with high adhesiveness |
abstract |
The invention discloses a method for preparing a resorcinol adhesive for tires with high adhesiveness, comprising the following steps: (1) preparing a resorcinol dispersion; (2) preparing a swollen product; (3) Post-treatment of the swollen product; (4) Homogeneous stirring; (5) Dehydration and drying. The polystyrene with low cross-linking degree of the present invention is not only easily penetrated by resorcinol and swells, but also can maintain the maximum swelling rate without being dissolved so as to maintain high viscosity, and combined with vinyl silicone oil emulsion to further improve the adhesive strength. In addition, the present invention also utilizes the free resorcinol in the contrast system of the sealing agent to carry out adsorption and blocking, so as to prevent its high temperature decomposition and reduce the smoke generation rate. |