Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_17a04f5a0c2ce082933c561e6a176e63 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2227 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2224 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2296 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5465 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 |
filingDate |
2019-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_19aa517d206db5d45974929c030995c2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b22111ac2594930c016062e440ce1ca6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d0ca230e99bd0ccdcbc719c54f93578b |
publicationDate |
2020-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-110791100-A |
titleOfInvention |
A kind of organosilicon high-strength anti-aging material containing modified graphene and preparation method thereof |
abstract |
The invention belongs to the field of organic silicon, and discloses an organic silicon high-strength anti-aging material containing modified graphene, which is characterized by comprising the following components in weight percentage: 25-50% of hydroxyl silicone oil; 2-5% of dimethyl silicone oil %; Nano Calcium Carbonate 0.1-3%; Silane-modified Graphene 2-6%; Flame Retardant Powder 5-15%; Hydrophobic Silica 4-8%; Crosslinking Agent 1-5%; Catalyst 0.01-0.05% ; The solvent is added to 100%; the crosslinking agent is composed of the following components in weight percentage: 80% of methyltributanone oximosilane; 20% of tetrabutanone oximosilane. After the material was modified by graphene, its strength and aging resistance were significantly improved. Meanwhile, the invention also discloses a preparation method of the material. |
priorityDate |
2019-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |