http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110746608-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2253-202 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02C20-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-151 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2387-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2220-4812 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-262 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G81-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G81-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L87-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-02 |
filingDate | 2019-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110746608-B |
titleOfInvention | Nitrogen-containing cyclodextrin polymer porous material and preparation method and application thereof |
abstract | The invention discloses a nitrogen-containing cyclodextrin polymer porous material and a preparation method and application thereof. Adding 15mmol of beta-cyclodextrin into 100-150 mL of organic solvent containing 54mmol of alkali under the inert gas atmosphere, fully stirring and dissolving to obtain a solution 1, placing the solution 1 in an ice-water bath, dropwise adding 50mL of a solution 2 into the solution 1, and reacting at the temperature of 0-5 ℃ for 12 hours to obtain a reaction solution 1; dissolving 7.5mmol of polyethyleneimine into 50-75 mL of organic solvent to obtain a solution 3, dropwise adding the solution 3 into the reaction solution 1, heating to 80-100 ℃, and continuing to react for 12-24 hours to obtain a reaction solution 2; and cooling the reaction liquid 2 to room temperature, filtering, washing solid powder obtained by filtering, and drying to obtain the nitrogen-containing cyclodextrin polymer porous material. The preparation method is simple and low in cost, and the obtained material can realize CO by utilizing hydroxyl of cyclodextrin and nitrogen-containing functional groups of organic amine 2 High adsorption capacity and selectivity, large adsorption capacity, high selectivity, easy regeneration and the like. |