http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110743585-B

Outgoing Links

Predicate Object
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-38
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-308
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-34
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-22
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J21-063
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1004
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J21-18
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-30
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-38
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-22
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J21-18
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J21-06
filingDate 2019-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2022-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationDate 2022-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-110743585-B
titleOfInvention Preparation method of graphene-based nano titanium dioxide sheet for enhancing visible light catalysis
abstract The invention discloses a preparation method of a graphene-based nano titanium dioxide sheet for enhancing visible light catalysis, which comprises the following steps: (1) adding graphene oxide into the amino-terminated polymer solution, and carrying out ultrasonic treatment for 0.5-2h to obtain A; (2) mixing hydrofluoric acid and a titanium dioxide precursor to obtain B; (3) mixing A and B, stirring for 20-40min, and carrying out solvothermal reaction to obtain C; (4) and C, cooling, washing and drying to finally obtain the graphene-based nano titanium dioxide sheet. According to the invention, a one-step solvothermal method is adopted, an amino-terminated polymer is taken as a solvent, graphene oxide is reduced, a (001) -surface-exposed nano titanium dioxide sheet is generated in a co-located mode, a new Ti-C chemical bond is formed in the growth process, the connection between the nano titanium dioxide sheet and the graphene oxide is enhanced, the forbidden bandwidth of the titanium dioxide is narrowed, and the photocatalytic degradation effect of the titanium dioxide under the visible light condition is obviously improved.
priorityDate 2019-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID407275646
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457280313
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID21801
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559581
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707770
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6547
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID414859283
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14917
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID297
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID454228257
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23673835
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID702
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID26042
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419538410

Total number of triples: 44.