http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110735040-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_531333fc5962ee597e26def2814324d1 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B7-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B47-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B47-00 |
filingDate | 2018-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0abb5f5efa716ea2ac8a18c97ea1fc9a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c910475765d570a8a0115c9f7de3a8b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c075eaf9a439f26108782c01ba2c081 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45ff52513808897e5c7763b334b2a1cc |
publicationDate | 2020-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110735040-A |
titleOfInvention | Electrolytic metal manganese waste residue treatment method |
abstract | The invention relates to a method for treating electrolytic manganese metal waste residue, which comprises the following steps: A. limestone is roasted to obtain quicklime and carbon dioxide; B. electrolytic metal manganese waste residue is slurried, leached, lime powder is added, and ammonia gas is recovered; the pH of the solution is adjusted to 6.0-6.4, Remove iron oxide, filter press to obtain filter press block A and filter press A, wash filter press block A with water and filter press to obtain filter press block B and filter press B; adjust the pH of filter press A to 11.5-12, filter press, Obtain filter press block C and press filtrate C; C. add silicon dioxide, calcium oxide, alumina, iron oxide in filter press block B, dry, pre-decompose, calcine to obtain cement clinker; D. filter press block C Slurrying, leaching, adjusting pH to 6.0‑6.4, removing impurities, standing, and pressure filtration to obtain filter press block D and pressure filtrate D, adding ammonia water to pressure filtrate D to adjust pH to 8.8‑9, and continuing to add ammonia solution to adjust pH to 11.4‑11.8. The method realizes the recycling and reuse of resources. |
priorityDate | 2018-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |