http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110643179-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-3009 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L81-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-1515 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 |
filingDate | 2019-11-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110643179-B |
titleOfInvention | High-toughness wear-resistant polyphenylene sulfide composite material |
abstract | The invention relates to the technical field of high polymer materials, in particular to a high-toughness wear-resistant polyphenylene sulfide composite material. Comprises the following components in parts by weight: 30-70 parts of polyphenylene sulfide, 0.2-0.5 part of antioxidant, 1-3 parts of lubricant, 5-15 parts of toughening agent, 5-15 parts of wear-resistant assistant and 20-40 parts of glass fiber. The high-toughness wear-resistant polyphenylene sulfide composite material is prepared from polyphenylene sulfide, glass fibers and the like, the polyphenylene sulfide and the glass fibers have a good synergistic effect, and the antioxidant is added, so that the aging resistance of the composite material is improved, and the service life of the composite material can be prolonged; the strength and toughness of the composite material are improved by adding the compatible toughening agent; the wear-resistant additive is added, so that the wear resistance of the composite material is improved; the addition of the glass fiber improves the strength, toughness and wear resistance of the composite material, and the prepared high-toughness wear-resistant polyphenylene sulfide composite material has high strength, good toughness, excellent shock resistance and better wear resistance. |
priorityDate | 2019-11-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |